New Metal-Containing Acrylated Oligomers Impart Excellent Adhesion in Coatings
Recently, Sartomer chemists developed a series of organic metal acrylate oligomers that are soluble in most monomers, leading to higher formulation capabilities. These new oligomers were studied in various applications. Due to their hydrophobic nature, the metal-containing oligomers can be used at high levels in standard radiation-curable formulations. They have also been shown to promote adhesion to metal and glass.
It is anticipated that these products, and products based on other metals, will demonstrate high-value performance, such as conductivity, high refractive index, anti-fungal properties, and more. Because of these physical properties, formulators will now be able to create coatings with excellent adhesion that are clear and flexible, and have anti-fungal properties.