Effect Pigments EMD Chemicals Inc. Xirallic® T60-25 SW Cosmic Turquoise effect pigment is available with a unique, SW chrome-free exterior durable treatment suitable for applications such as automotive, architectural, electronics and accessories. Its narrow particle size distribution leads to good application results in most paint systems. Visit www.emdpigments.com.
Defoamers Octel Performance Chemicals, Inc. Octafoam® E-314 and Octafoam E-316 dispersible oil-based defoamers have been developed for aqueous adhesive formulations. Octafoam G-408 and Octafoam G-409 glycol-based defoamers have been developed for use in water-reducible industrial coatings. Octafoam G-409 is particularly recommended for use in the grind phase. Octafoam N-209 non-dispersible oil-based defoamer was developed as a grind-phase defoamer for architectural paints. Octafoam N-213 is a zero-VOC defoamer for use in low- or zero-VOC systems. It is also food grade. Octafoam S-606 is a silicone emulsion food-grade defoamer with extremely high efficiency. Call 800/515.2436.