ASTM Coatings Committee to Develop Color Guide, Seeks Project Participants
WEST CONSHOHOCKEN, PA - ASTM Committee D01 on Paint and Related Coatings, Materials and Applications has issued an invitation to users of color specifications to participate in the development of a standard related to how a supplier and customer set a color specification for a material.
The proposed guide will assist technicians in establishing numerical (instrumental) tolerances for color and provide standards of ideal color for raw-material suppliers, coatings producers, or pigment suppliers setting color specifications, ASTM said.