PITTSBURGH - Bayer Corp.'s Coatings and Colorants Division announced plans to consolidate polyester resins manufacturing at the company's New Martinsville, WV, and Columbus, GA, production sites and close its plant at Hicksville, NY, by the end of this year.
The company said the moves are part of an ongoing site-consolidation program designed to eliminate excess capacity and reduce costs.