ASTM Coatings Panel Seeks Participants for ISO Test-Method Review
WEST CONSHOHOCKEN, PA — ASTM Committee D01 on Paints and Related Coatings, Materials and Applications issued an invitation to volunteers and other participants for the review and critiquing of ISO test methods for paint and varnishes.
The committee serves as the U.S. Technical Advisory Group (TAG) to a subcommittee of the International Organization for Standardization (ISO) that is involved in general test methods for paint and varnishes. ASTM is scheduled to host ISO subcommittee meetings on June 11-13 in Pittsburgh.