EPA Recognizes Use of Non-Chromate Coatings for Aircraft-Finishing Applications
PHOENIX-Pantheon Chemical Co. said the Science and Engineering Laboratories at Hill Air Force Base in Ogden, UT, have been named a recipient of the EPA Regional Administrative Award for Environmental Excellence as a result of the Air Force base's action in eliminating the use of chromated conversion coatings for aircraft-finishing operations.
The EPA award is presented to individuals and groups who have made "exceptional contributions to the protection of human health and the environment."