LANGELSHEIM, Germany - Heubach GmbH announced the acquisition of certain assets of Bayer AG's Lightfast Pigment business, including manufacturing equipment and intellectual property. The purchase does not include a complex inorganic color pigment plant in Leverkusen, Germany.
Products include inorganic pigments such as titanate yellows, cobalt blues, cobalt greens and spinell blacks used in coatings and plastics.