Kerr-McGee Completes Buyout of European TiO<sub>2</sub> Plants
OKLAHOMA CITY — A German subsidiary of Kerr-McGee Chemical LLC has acquired Bayer AG’s 20% stake in Kerr-McGee’s titanium dioxide (TiO2) pigment plants in Uerdingen, Germany, and Antwerp, Belgium, for 25 million euros, or approximately $22 million (U.S.)
Kerr-McGee acquired 80% of the Uerdingen and Antwerp pigment facilities in 1998, with an option to acquire the remaining 20% from Bayer. The two plants have an annual production capacity of approximately 130,000 metric tons.