WILMINGTON, DE - DuPont White Pigment & Mineral Products, the world's biggest supplier of titanium dioxide (TiO2) pigments, announced a change in the business's name to DuPont Titanium Technologies.
The new name reflects the business's variety of products and services, said the unit's vice president and general manager, Jeffrey L. Keefer.