PVD Aluminum Pigments: Superior Brilliance for Coatings & Graphic Arts
The history of metal pigments has its origin in the gold leaf manufacturing that was in production about 1,000 years BC. Ancient Egyptians knew the art of working gold into very thin sheets, and how to use those sheets for the decoration and ornamentation of wood, bone, and other materials.
Over time, this art spread to China, India and Europe, where a trade was quickly developed.