Prepolymer GE Advanced Materials-Silicones SPUR+* Y-15735 LM prepolymer is a low-modulus member of a new family of next-generation silylated polyurethane resins for adhesives, sealants and coatings applications. SPUR+ prepolymers offer exceptional adhesion to a wide range of porous and non-porous substrates, including metals, glass, ceramics and plastics - even wet, primerless concrete. Specifically, SPUR+ Y-15735 LM prepolymer is three times as fast in tack-free time and enhances deep-section cure under ambient conditions by about 50 percent, compared to similar resins with earlier silane end capping technologies. Visit www.ge.com. (*SPUR+ is a trademark of General Electric Company.)