The Labstar(r) is capable of processing batch sizes from 1 L to over 1 gal, and operates in both horizontal and vertical positions. The mill is also engineered for CIP processes, making batch changes and clean-up fast and easy. A variable speed drive through frequency inverter and optional PLC controls are available. For more information, phone 610/363.8010; e-mail grinding@netzschusa.com; or visit www.netzschusa.com.