Powder Application Methods Offer Variety and Versatility in Coating Options
The Powder Coating Institute’s Jeff Palmer gives an overview of the latest advancements in powder application.
Some woods and wood products have enough moisture content to provide sufficient conductivity and can be coated directly. Wood parts can be blown off with compressed air to eliminate any surface contaminants. To enhance electrostatic attraction, wood can be pretreated with a liquid coat to improve adhesion, and the part can be preheated.