California Paints Fres~Coat Exterior Paint Gets Top Ranking by Consumer Magazine
ANDOVER, MA - California Paints' "Fres~Coat" Velvet Flat House Paint earned the top ranking among exterior paint for 2004 by Consumer Reports magazine. Also scoring high rankings for exterior paint performance were Pratt & Lambert's "Accolade" eggshell paint and Glidden's "Endurance" semigloss paint.
Consumer Reports published performance results for premium paints and stains in its June edition. Among the stains evaluated, the top scores were posted by PPG's Olympic Premium 596XX, Sherwin-Williams' Woodscapes Solid A15 and Behr Plus 10.