Krasol Prepolymers For Moisture- and Corrosion-Resistant Coatings
There are different types of metal corrosion and also different solutions to the corrosion problem. One of the most effective methods of corrosion control is the use of protective coatings. The protection of metal structures and poles against corrosion can be met by using one-component polyurethane coatings. Binders for these coatings are often isocyanate prepolymers based on the reaction of a difunctional polyol with an aromatic or an aliphatic diisocyanate.