The RX Firefly ultraviolet (UV) Light System is based on the company's SLM (Semiconductor Light Matrix) technology. The system is designed as a small-format/high-intensity UV light source with a 20mm diameter target spot size and a typical peak intensity of greater than 1.5W/cm2. This is equivalent in useful UV output seen at the work surface to that of many mercury vapor arc lamp sources, making the RX Firefly product ideal for small-area and spot-cure applications. Visit www.phoseon.com/products.