The award was accepted by Dennis Kovalsky, PPG vice president, automotive OEM coatings; Bo Andersson, GM vice president, global purchasing and supply chain; and James Haverland, GM director, paint and polymers engineering.
The color-specific powder primer has a high-gloss finish and is tinted to match a vehicle's paint color. It provides a finished look for hard-to-paint areas such as inner surfaces of trunk and engine compartments, according to Rick Tansey, technical manager, PPG.