Design of Wetting and Dispersing Additives for Selected Pigments
Changing the vinyl polyether design (e.g., using hydrophobic alkylene oxide monomers) can make the polyethers compatible with different kinds of pigment surfaces.
Model structures from these different synthetic groups were compared in application tests and analytical measurements made for their pigment stabilization performance (see Table 1).