Performance properties have been determined using model formulations based on
UV PUDs and standard oligomers diluted with butyl acetate. Mechanical
properties and chemical resistance of UV PUDs are similar or better than those
obtained with standard oligomers, with the additional benefit of physical
drying that leads to a tack-free film before UV cure while minimizing VOC
generation.