A Novel Micronized High-Performance Rutile
Yellow: New Options – New Chances
By
optimizing the well-known chrome and nickel titanium yellow chemistries, which
exhibit outstanding fastness and durability, a new class of pigments has been
obtained offering a versatile tool for formulating economic and innovative
coatings.