Coating’s polymers poke holes in the
membranes that surround influenza viruses.
“Because
of the limited efficacies with existing (flu) vaccines and antivirals, there’s
room for other, complementary approaches,” said Chen, one of the authors of a
report on the new material that appeared Nov. 13, 2006 in the online edition of
the Proceedings of the National Academy of Sciences.