SouthWest NanoTechnologies Unveils Coatings Application Development Center
SouthWest NanoTechnologies Inc. (SWeNT), Norman, OK, a manufacturer of single-wall and specialty multi-wall carbon nanotubes, in partnership with Chasm Technologies Inc. (Chasm), a consulting firm specializing in nanomaterials and thin film coating and patterning, have established a carbon nanotube coatings application development center at Chasm’s facility located in the Boston area.