PPG White Paper Compares Polysiloxane Coatings With Traditional Coatings
PPG Industries’ protective and marine coatings (PMC) business has published a white paper comparing the performance of polysiloxane coatings to that of traditional epoxy/urethane and epoxy/silicone-alkyd coatings.