This is based on an actual example: Coating "A"-a "traditional" coating-has total solids by volume of 32.62% (the rest being largely eventual waste) and costs just $13.67 per gallon.
Coating "B" has total solids by volume of 99.69% but costs over twice as much, or $35 per gallon.