Powder coatings from
cyclic carbonate functional polymers and amine carbamate salts
U.S. Patent 6,339,129
Issued: January 15, 2002
Inventors: Webster, Dean Charles
Assigned to: Eastman Chemical Co.
Curable coating compositions for powder coatings are disclosed, which are
composed of a cyclic carbonate functional polymer and a carbamate salt of a
multifunctional amine.