Peridium Powder Coatings
are manufactured by using a process that utilizes fourth generation German and
Swiss premixing, extruding and grinding equipment, which offers production
control and efficiency. A computer-aided laser defraction unit measures powder
particle size and particle distribution, which centers around tightly
controlled, smaller average particle size. Peridium Powder Coatings have high
first-pass transfer efficiency and electrostatic wrap for powder coating end
users. The coatings are available in a wide variety of colors, glosses, finishes
and chemistries. Peridium Powder Coatings are offered in epoxy, epoxy-polyester
hybrids, TGIC polyester and urethane polyester formulas. Diamond Vogel Paints
800-728-6435