Extruder
Offers Low-Torque Compounding
The Compex
Multi-Process Compounder is designed for the low-torque mixing of powder coating
formulations. It is available in screw diameters from 25 to 85 mm.
Nonintermeshing and back-flow elements work together to thoroughly mix polymers.
The smooth, continuous torque minimizes shear force and allows gentle and
uniform incorporation of additives and temperature-sensitive materials. Berstorff
Corp. 859-283-7484
Extruder
Features Side-Feed System
The PCS
extruder for powder coating manufacturing incorporates a side-feed system that
optimizes feeding of premix, fines and rework. It is available in 8 L/D and 11
L/D working lengths and five screw diameters ranging from 46 to 140 mm. Users
benefit from the extruder's wide processing window, increased screw speed, good
thermal control and high throughput rates. Buss
America Inc. 630-307-9900