Flow
Modifier Enhances Surface Appearance
Modarez MFP-A25P flow modifier for powder coatings was designed to address the
surface imperfections, such as orange peel and craters, seen in
low-temperature-cure systems for wood and plastic substrates. This silicone-free
polymer works well in TGIC polyesters, epoxy hybrids and GMA-acrylic systems,
and it can be used in both industrial and automotive formulations. It will not
yellow during overbake conditions and delivers enhanced flow, smoothness and
recoatability. Synthron Inc. 828-437-8611
Texturing Agent Reduces
Gloss
PowderTex 61 crystalline fluoropolymer texturing agent produces consistent,
reproducible textures in a wide range of powder coatings. It provides good gloss
reduction and texture appearance at low concentrations. This processed
polytetrafluoroethylene produces satin gloss and controlled orange peel-type
textures in general metal finishes and coatings for OEM and aftermarket
automotive parts, farm equipment and electronics. Shamrock Technologies 800-349-1822