A powder coating method
includes applying an antistatic material to the surface of an electrically
nonconducting substrate. The antistatic material is preferably a fatty amine
salt and is applied by spraying. A flow of electrostatically charged powder
particles is directed toward the substrate to form a powder coating on the
substrate, and the powder coating is thereafter cured.