Tests performed around the perimeter of a “painted” sensitive compartmented information facility (SCIF) yielded successful results for the protection of wireless devices and other electronic equipment within the structure. The tests confirmed that wireless transmission of information can be protected from unauthorized access by the use of a new coating from EM-SEC Technologies, LLC.