Finishing professionals who apply CARC should have a thorough working knowledge of the two main specifications pertinent to CARC: TT-C-490, which covers Cleaning and Pre-Treatments; and MIL-DTL-53072, which addresses Application Procedures and Quality Control. Designed to be used in conjunction with each other, these two specifications allow for a full understanding of the system.