UCECOAT® 7631 waterborne UV curable resin from Cytec Industries Inc. is designed for use in topcoats on outdoor wood joinery. The aliphatic polyurethane dispersion reportedly offers superior weathering resistance, as well as outstanding chemical and mechanical resistance.