This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Home » MATERIALS: Hex-Free Conversion Coating Achieves QPL Status - Posted 7/25/07
Carolina Process Control, a distributor of metal finishing chemicals and equipment, has received approval under the government’s Mil Spec of MIL-DTL-81706B for chemical conversion coatings for its Luster-On product known as “Aluminescent.” The product is now officially listed on the Qualified Products List (QPL) pertaining to chemical conversion materials for coating aluminum and aluminum alloys.