The application environment typically is the most important factor in how well a coating can shield an offshore oil platform from corrosion above the splash zone. However, it is not always possible to apply the coating in the “optimal” environment or to set aside enough time for the application. Advances in organic zinc primers are reducing the application time of coatings on offshore oil platforms compared to conventional inorganic zinc systems, without compromising performance.