Needle Roller Bearings Co. Ltd (NBR), a leading manufacturer of needle roller bearings targeted for use in motorcycle engines, outboard motors and other high rotational speed engines, has chosen Victrex plc’s VICOTE® 804 Blk coating to replace copper and silver plating. The coating is believed to reduce the wear on the outer surface of the roller bearing, and thus can enable longer life of the actual cage.