Innovative Roof Coating Provides Energy Savings - Posted 11/28/07
Rohm and Haas has updated the roof of its nine-story global headquarters with an advanced polymer elastomeric roof coating that reflects a broad spectrum of UV, visible and infrared light and emits nearly 90% of any absorbed heat, all of which contribute to the degradation of traditional roofing materials and the energy consumption of buildings.