Air Products Debuts Thermal Spray Cooling Technology - Posted 11/14/07
Air Products has introduced a new thermal spray cooling technology to the North American market that uses cryogenic nitrogen vapor (-320°F) to maintain part temperature during thermal spray coating applications. The company’s U.S. patent-pending technology makes high-quality thermal spray coatings possible by maintaining part temperature within a pre-defined narrow range, even for heat-intensive spraying processes. The technology can enable the user to apply coatings faster and at a lower cost than traditional cooling methods.