Bekaert to Sell Diamond-Like Carbon Coating Business - Posted 6/10/08
NV Bekaert SA plans to sell its Diamond-like Carbon (DLC) coating activities to Switzerland-based Sulzer. The DLC business is part of Bekaert’s advanced coatings business segment and hosts six production plants.