Peelable Paint Speeds Deployment of Military Vehicles - Posted 6/17/08
Changing paint schemes on military vehicles for rapid reaction deployment reportedly is quicker and more cost efficient using Intergard 10220, a peelable coating system developed by ANAC (Akzo Nobel Aerospace Coatings).