DALLAS- Oxea announced that it will increase list and off-list prices on a number of products.
Effective February 15, 2012, or as contracts allow, in the United States, Canada and Mexico, i/n butanol will increase $0.05/lb. (zone 1 list price of $1.58), i/n butyl acetate will increase $0.05/lb. (zone 1 list price of $1.36), n butyraldehyde will increase $0.05/lb. (zone 1 list price of $1.59), n propanol will increase $0.05/lb. (zone 1 list price of $1.35), and n propyl acetate will increase $0.05/lb. (zone 1 list price of $1.33).