Ecology Coatings, Inc., a leader in the discovery and development of nanotechnology-enabled, ultraviolet-curable advanced coatings, has developed a UV-curable coating to meet the rigorous requirements of the healthcare industry. The coating is applied to a multilayered paper, printable patient wristband and is benzophenone free − a request that is becoming a requirement within the food industry and is increasing in popularity within the healthcare sector.
“A major U.S. label manufacturer, searching for improved product performance, asked that we develop a UV-curable coating for patient identification wristbands used by their customers within the healthcare industry,” commented Ecology Coatings CEO Bob Crockett. “Sally Ramsey, our Vice President of Research and Development, worked with the manufacturer to understand the use, durability and longevity of the wristbands in a hospital. Based on the data gathered, Ramsey and her staff developed a coating that would be clear, glossy and resistant to water, blood, urine, betadine, alcohol, xylene, acetone, antimicrobial skin cleansers, chlorhexidine and a number of other common chemicals that could come in contact with patient wristbands.”