Demand is increasing for rich, classic black coatings for high-end products, particularly in consumer electronics such as computers and televisions; premium household products including countertop appliances, bath and kitchen fixtures; automotive interior and exterior accents and accessories; and in large coating services and electroplating operations.
Vapor Technologies, Inc., an industry pioneer in physical vapor deposition (PVD) thin-film coating systems for wide-ranging industrial and consumer product applications, has developed the first true black advanced low-temperature arc vapor deposition (LTAVD) coating