Sachtoperse Functionalized Pigments Provide Direct Chemical Bonding
INDIANAPOLIS - Sachtleben has expanded its Sachtoperse family of barium sulphate pigments to include new patented, functionalized pigments designed to optimize paint properties and meet new requirements in the coatings market.
“Developed in response to international demand, our new pigments are optimally tailored to their respective binder and designed to provide secure bonding between pigment and resin,” explained Milan W. Krumbe, Director Coatings of Sachtleben. “We refer to this bonding mechanism as ‘the octopus effect.’”