MAIA, Portugal - CIN, Iberia's leading paint and varnish company, has substantially reduced its environmental footprint by setting up a treatment unit for VOCs at its Maia industrial site and by developing more environmentally friendly solutions for its customers.
With an initial investment of EUR 700,000 in technology, CIN has achieved a more than 95 percent reduction in VOC emissions from the 40,000 cubic meters/hour of contaminated air produced by the industrial site in question.