At less than 340 g/L VOC, it complies with current Ozone Transport Commission (OTC) limits. Acrolon Ultra is optimized for brush and roll application and can be sprayed using airless or conventional spray equipment. It also provides a rapid return to service; the coating can be dry to the touch in as few as two hours after application.