Arkema Coating Resins Realigns Distribution in North America
CARY, NC - Arkema Coating Resins has realigned distribution of ENCOR®, NEOCAR®, SNAP® and Celocor® waterborne products in North America to better meet the needs of its customers. The company has announced distributors based on market and geography.
In the United States, Brenntag and Nexeo Solutions will distribute paint, coatings, adhesives and construction products. Products for inks and graphic arts will be distributed by Palmer Holland.