GEO Specialty Chemicals is exhibiting at the ECS for the first time following its acquisition of the Bisomer® Monomer business from BASF. GEO is featuring its expanded product offerings to the European coatings and adhesives market, in particular its novel TRI-REZ™ polyester and DMPA® polyols, and its extensive range of specialty acrylic monomers.
Bisomer BZMA (Benzyl Methacrylate) is the latest addition to the Bisomer range of specialty methacrylates. Its key properties of low viscosity, hydrophobicity and high refractive index make it ideal for a wide range of applications such as adhesives, composites, sealants and optical fibers. It is an excellent option for customers looking to reduce styrene from their formulations and it has good compatibility with unsaturated polyesters, vinyl esters, acrylic and methacrylic monomers.