Nano Labs Corp. Develops New Technology in Self-Cleaning Coating
DETROIT - Nano Labs Corp. announced the development of a new self-cleaning paint that degrades pollutants through a proprietary nanoparticle compound and natural light.
The eco-friendly coating will help exterior surfaces maintain performance and appearance standards for much longer periods of time.