Ashland Receives Ringier 2013 Coatings Technology Innovation Award
SHANGHAI - Ashland Specialty Ingredients, a commercial unit of Ashland Inc., Covington, KY, recently received a Ringier 2013 Coatings Technology Innovation Award for its NatrosolTM Performax paint thickening technology. It is the third consecutive year Ashland has won the innovation award.
The Ringier Technology Innovation Awards recognize those who have made significant contributions for the advancement of the industry through technical innovation, improved productivity, economic efficiency and market opportunity creation. Ringier Technology Innovation Awards are regarded as one of the most important awards in China's coating industry.