FLORHAM PARK, NJ – Troy Corp., Florham Park, NJ, has won the Ringier Technology Innovation Award for Additives in China’s coatings industry. The award was created to honor those companies that have introduced a new product, technology, or process that advances the coatings industry in China, such as improving efficiency, cost performance, or environmental responsibility. A panel of industry experts evaluated new technologies that debuted and were made commercially available between 2011 and 2013.
Troy was selected for an Additives award for its introduction of Polyphase® 2167, an innovative, zero-VOC broad-spectrum dry-film preservative that not only is highly effective against fungi and yeast, but also creates an antibacterial surface through a unique immobilization technology.